        | Title: | Hard Coating Treatment of Aluminum AlloysTeflon-Impregnated or Codeposited | 
      
        | Number: | AMS 2482 | 
      
        | Revision: | C | 
      
        | Scope: | This specification establishes the engineering requirements for producing a hard Teflon-impregnated or codeposited Teflon-aluminum oxide coating on aluminum alloys and properties of such coatings.  This process has been used typically to increase, by formation of a dense, Teflon-impregnated aluminum oxide or codeposited Teflon-aluminum oxide layer, surface hardness and resistance to abrasion and corrosion of aluminum alloy parts containing, in general less than 5% copper or 8% silicon or a total of 8% of both.  Alloys with higher silicon content alone can be coated satisfactorily with proper precautions in processing.  careful consideration should be given to the use of this process on highly-stressed parts because of the resultant marked lowering of fatigue performance, and on parts with sharp corners and edges where chipping may result. | 
      
        |  |  | 
      
        | 
            
              | Classification: |  |  
                | Types                | The processes covered by this specification are classified as follows: |  | 
      
        |  |  | 
      
        | 
            
              | Details | Description | Can Do |  
                | Type 1 | Teflon-impregnated aluminum oxide | Yes |  
                | Type 2 | Codeposited Teflon and aluminum oxide. | No |  | 
      
        |  | 
      
      
        |  | 
   
      
        |  | 
      
        |  |