Title: |
Hard Coating Treatment of Aluminum AlloysTeflon-Impregnated or Codeposited |
Number: |
AMS 2482 |
Revision: |
C |
Scope: |
This specification establishes the engineering requirements for producing a hard Teflon-impregnated or codeposited Teflon-aluminum oxide coating on aluminum alloys and properties of such coatings. This process has been used typically to increase, by formation of a dense, Teflon-impregnated aluminum oxide or codeposited Teflon-aluminum oxide layer, surface hardness and resistance to abrasion and corrosion of aluminum alloy parts containing, in general less than 5% copper or 8% silicon or a total of 8% of both. Alloys with higher silicon content alone can be coated satisfactorily with proper precautions in processing. careful consideration should be given to the use of this process on highly-stressed parts because of the resultant marked lowering of fatigue performance, and on parts with sharp corners and edges where chipping may result. |
|
|
Classification: |
|
Types |
The processes covered by this specification are classified as follows: |
|
|
|
Details |
Description |
Can Do |
Type 1 |
Teflon-impregnated aluminum oxide |
Yes |
Type 2 |
Codeposited Teflon and aluminum oxide. |
No |
|
|
|
|
|